Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
NYCOA 5033 HST 33% Glass-Fiber Reinforced, Heat Stabilized, Translucent Nylon 66 Resin NYCOA 5033 HST is a 33% glass fiber reinforced, heat stabilized, translucent Nylon 66 resin used for injection molding. It has been specifically formulated for see through storage tanks for automoti.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2203-25 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP SFP36 PA12 LNP* LUBRICOMP* SFP36 is a compound based on Nylon 12 resin containing 30% Glass Fiber 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes.. |
|||
Izod Impact, Unnotched | 9.98 J/cm @Temperature 23.0 °C |
18.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp YF005 LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 9.98 J/cm | 18.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched | 9.98 J/cm | 18.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 9.98 J/cm | 18.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D256 |
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
Izod Impact, Unnotched | 10.0 J/cm | 18.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXN PA 66 LNP* THERMOCOMP* RF007SXN is a Hydro-Stable, 35% Glass Fiber reinforced compound based on Nylon 66. Added features of this grade include: Heat Stabilized, NSF Listed. |
|||
Izod Impact, Unnotched | 9.98 J/cm @Temperature 23.0 °C |
18.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |