Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.94 J/cm @Temperature 23.0 °C |
5.51 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp AF002L ABS (Asia Pacific) LNP* Thermocomp* AF002L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC.. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Izod Impact, Unnotched | 2.94 J/cm @Temperature 23.0 °C |
5.51 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp AF002L ABS LNP* Thermocomp* AF002L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC.. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.10% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 2.94 J/cm | 5.51 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 212 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |