Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.56 J/cm

@Temperature 23.0 °C
6.67 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT
LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.