Polymer Property : Izod Impact, Unnotched = 3.80 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.03 J/cm
3.80 ft-lb/in
Reliance Industries Polypropylene - Suzorite mica (untreated) filler
Information provided by Reliance Industries
Izod Impact, Unnotched 2.03 J/cm
3.80 ft-lb/in
ASTM D4812
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
Izod Impact, Unnotched 2.03 J/cm

@Temperature -40.0 °C
3.80 ft-lb/in

@Temperature -40.0 °F
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at..
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6/6 GB30 FR 30% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearance: BlackTPCI# ..
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GB20 L 20% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GB10 L 10% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GB15 15% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GB20 L BK 20% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GB25 L BK 25% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GB30 L 30% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.17 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PPS/F GF30 TL15 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackIn..
Izod Impact, Unnotched 2.03 J/cm

@Thickness 3.18 mm
3.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..