Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.01 - 21.4 J/cm
15.0 - 40.0 ft-lb/in
ASTM D256
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Izod Impact, Unnotched 8.01 - 21.4 J/cm
15.0 - 40.0 ft-lb/in
ASTM D256
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..