Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.23 J/cm

@Temperature 23.0 °C
9.80 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Izod Impact, Unnotched 5.23 J/cm

@Temperature 23.0 °C
9.80 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific)
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX01303C PC
LNP STAT-KON* DX01303C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66
LNP* STAT-KON* RE004 is a compound based on Nylon 66 resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF0039S PA 66
LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend
LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific)
LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
At 73°F; ASTM D256
Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene
Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l..
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 131 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 132 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 662 Nylon 6, Glass Bead Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Glass Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Lubrilon® 635 Nylon 6/6, Carbon Fiber/PTFE Filled, Proprietary Lubricant Package
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..