Polymer Property : Izod Impact, Unnotched = 5.86 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.13 J/cm

@Temperature 23.0 °C
5.86 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS
LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am..