Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.60 - 5340 J/cm | 3.00 - 10000 ft-lb/in | Average value: 2.14 J/cm Grade Count:10 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Unnotched | 6.41 - 5340 J/cm | 12.0 - 10000 ft-lb/in | Average value: 12.8 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Unnotched | 0.961 - 5340 J/cm | 1.80 - 10000 ft-lb/in | Average value: 0.969 J/cm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Izod Impact, Unnotched | 4.80 - 5340 J/cm | 8.99 - 10000 ft-lb/in | Average value: 4.80 J/cm Grade Count:3 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 6.94 - 5340 J/cm | 13.0 - 10000 ft-lb/in | Average value: 6.94 J/cm Grade Count:14 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched | 10.7 - 5340 J/cm | 20.0 - 10000 ft-lb/in | Average value: 16.4 J/cm Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Unnotched | 0.801 - 5340 J/cm | 1.50 - 10000 ft-lb/in | Average value: 6.47 J/cm Grade Count:296 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 10.5 J/cm Grade Count:13 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 11.7 - 5340 J/cm | 22.0 - 10000 ft-lb/in | Average value: 13.4 J/cm Grade Count:7 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 2.40 - 5340 J/cm | 4.50 - 10000 ft-lb/in | Average value: 6.94 J/cm Grade Count:13 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 2.08 - 5340 J/cm | 3.90 - 10000 ft-lb/in | Average value: 7.33 J/cm Grade Count:55 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 8.10 J/cm Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Unnotched | 0.534 - 5340 J/cm | 1.00 - 10000 ft-lb/in | Average value: 9.81 J/cm Grade Count:19 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 8.92 J/cm Grade Count:19 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Izod Impact, Unnotched | 4.27 - 5340 J/cm | 8.00 - 10000 ft-lb/in | Average value: 8.81 J/cm Grade Count:4 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Unnotched | 1.39 - 5340 J/cm | 2.60 - 10000 ft-lb/in | Average value: 11.7 J/cm Grade Count:35 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Unnotched | 0.481 - 5340 J/cm | 0.900 - 10000 ft-lb/in | Average value: 4.50 J/cm Grade Count:45 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched | 10.7 - 5340 J/cm | 20.0 - 10000 ft-lb/in | Average value: 21.9 J/cm Grade Count:19 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Izod Impact, Unnotched | 4.64 - 5340 J/cm | 8.69 - 10000 ft-lb/in | Average value: 8.60 J/cm Grade Count:47 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Unnotched | 2.14 - 5340 J/cm | 4.00 - 10000 ft-lb/in | Average value: 3.99 J/cm Grade Count:6 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Unnotched | 10.7 - 5340 J/cm | 20.0 - 10000 ft-lb/in | Average value: 12.0 J/cm Grade Count:5 |
Overview of materials for Nylon 11 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 10.7 - 5340 J/cm | 20.0 - 10000 ft-lb/in | Average value: 42.2 J/cm Grade Count:4 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Izod Impact, Unnotched | 0.300 - 5340 J/cm | 0.562 - 10000 ft-lb/in | Average value: 0.300 J/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Izod Impact, Unnotched | 6.41 - 5340 J/cm | 12.0 - 10000 ft-lb/in | Average value: 6.41 J/cm Grade Count:3 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Unnotched | 20.3 - 5340 J/cm | 38.0 - 10000 ft-lb/in | Average value: 21.0 J/cm Grade Count:16 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched | 7.35 - 5340 J/cm | 13.8 - 10000 ft-lb/in | Average value: 12.2 J/cm Grade Count:46 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched | 1.87 - 5340 J/cm | 3.50 - 10000 ft-lb/in | Average value: 6.03 J/cm Grade Count:136 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Unnotched | 0.801 - 5340 J/cm | 1.50 - 10000 ft-lb/in | Average value: 8.47 J/cm Grade Count:46 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched | 1.33 - 5340 J/cm | 2.50 - 10000 ft-lb/in | Average value: 4.39 J/cm Grade Count:41 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |
|||
Izod Impact, Unnotched | 1.60 - 5340 J/cm | 3.00 - 10000 ft-lb/in | Average value: 4.74 J/cm Grade Count:42 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |