Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.56 J/cm @Temperature 23.0 °C |
6.67 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |