Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS PC+ABS Blend with 20% Glass Reinforce. High heat resistance; Excellent balance strength/rigidity; Good impact/appearance. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UL002S PPA LNP* LUBRICOMP* UL002S is a compound based on Polyphthalamide resin containing 10% PTFE. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 4.53 J/cm | 8.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific) LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release. |