Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 11.20 MPa | 1625 psi | DCBP Cure |
Shin-Etsu Silicones KE-581U Silicone Elastomer KE581U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |
|||
Tensile Strength at Break | 11.20 MPa | 1625 psi | DCBP Cure |
Shin-Etsu Silicones KE-551U Silicone Rubber KE551U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |
|||
Tensile Strength at Break | 11.20 MPa | 1625 psi | DCBP Cure |
Shin-Etsu Silicones KE-571U Silicone Elastomer KE571U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |