Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.20 MPa | 1330 psi | Rate of 50 mm/min; ASTM D 638 |
NOVA Chemicals Surpass® IFs730-R Octene sMDPE Food Packaging Lid Resin IFs730-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Tensile Strength at Break | 9.17 MPa | 1330 psi | |
Shin-Etsu Silicones KE-961TU Silicone Elastomer KE961 TU is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).P.. |
|||
Tensile Strength at Break | 9.20 MPa | 1330 psi | ISO R 527 |
Stir SpA PVGUM 34 ATC UV (PVC) Application: Legging boot for dairy useInformation provided by STIR SpA |
|||
Tensile Strength at Break | 9.17 MPa | 1330 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 9.17 MPa | 1330 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4675A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 9.17 MPa | 1330 psi | ASTM D412 |
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 9.20 MPa | 1330 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 85 A.1 TPE-S, Shore A85, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 9.20 MPa | 1330 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to create multilayer constructions offering bonding to textiles,.. |