Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PC-15CF-15GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | |
Indium Corp. Indalloy 200 Pure Gold Information Provided by Indium Corporation |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
Techmer ES Plaslube® J-1/CF/10/TF/20 BK PA66 |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
Sumitomo Bakelite North America EM 7302 Hardware Grade Epoxy Long fiberglass reinforced epoxy molding compound which features high strength and toughness for structural components. This compound is designed for applications requiring Mil-M-46069 certificatio.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6 7500 TF 20 GF 20 Polyamide 6, 20% PTFE chemically bonded 20% glass fiber reinforced Description: Medium viscosity PA 6, 20% PTFE chemically bonded and 20% glass fiber reinforced, good flowability, good impact resistance and bright natural color.Application: For molding parts with.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |