Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 120 - 140 MPa | 17400 - 20300 psi | ASTM D683 |
Loxim 230 12V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Tensile Strength at Break | 110 - 140 MPa | 16000 - 20300 psi | ASTM D638 |
Adamas Rixon 130 PEEK, 30% Carbon Filled Information provided by Adamas, HPM |