Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 2.48 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 101 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Superior tensile and shear strengths, well suited for metal bondingLow gap fill. Methyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substr..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 10 s set time
Elmer's Products Aron Alpha® 102 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Superior tensile and shear strengths, well suited for metal bondingMedium gap fill. Methyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous sub..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 201 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 10 s set time
Elmer's Products Aron Alpha® 202 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 3 s set time
Elmer's Products Aron Alpha® 202F Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 25 s set time
Elmer's Products Aron Alpha® 203 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair o..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 212E Cyanoacrylate Adhesive (Industrial Krazy Glue™)
For clean, fast applications. Best for high speed automated assembly.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous s..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 1 s set time
Elmer's Products Aron Alpha® 221F Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 232 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 241F Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 253TX Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 401X Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Engineered for high temperature and high impact resistance.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. Ve..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 10 s set time
Elmer's Products Aron Alpha® 402X Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Engineered for high temperature and high impact resistance.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. ..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 30 s set time
Elmer's Products Aron Alpha® 403TB Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 25 s set time
Elmer's Products Aron Alpha® 403X Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Engineered for high temperature and high impact resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. V..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 15 s set time
Elmer's Products Aron Alpha® 432TB Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 15 s set time
Elmer's Products Aron Alpha® 432TW Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® GEL 10 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Tensile Strength at Break 2.48 MPa
360 psi
(20 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ UL 40028CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 40028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent..
Tensile Strength at Break 2.48 MPa
360 psi
(20 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ UL 40028EM1 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 40028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 10 s set time
Elmer's Products Aron Alpha® 241 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 241E Cyanoacrylate Adhesive (Industrial Krazy Glue™)
For clean, fast applications. Best for high speed automated assembly.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous subs..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 5 s set time
Elmer's Products Aron Alpha® 252E Cyanoacrylate Adhesive (Industrial Krazy Glue™)
For clean, fast applications. Best for high speed automated assembly.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous sub..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 3 s set time
Elmer's Products Aron Alpha® 252F Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Tensile Strength at Break 2.48 MPa
360 psi
JRF- 72 hrs @ 60°C, and Air Drying - 72 hrs @ 49°C, and 7 days @ 121°C
3M AC-236 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Tensile Strength at Break 2.48 MPa
360 psi
JRF- 72 hrs @ 60°C, and Air Drying - 72 hrs @ 49°C, and 7 days @ 121°C
3M AC-236 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t..
Tensile Strength at Break 2.48 MPa
360 psi
JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C + 24 hrs @ 49°C + Std Heat Cycle; AMS3276
3M AC-275 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Tensile Strength at Break 2.48 MPa
360 psi
JRF-12 days @ 60°C + 60 hrs @ 71°C + 6 hrs 82°C + 24 hrs @ 49°C + Std Heat Cycle; AMS3276
3M AC-275 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 30 s set time
Elmer's Products Aron Alpha® 453TB Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
Tensile Strength at Break 2.48 MPa
360 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL 0141-115 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco..
Copyright © lookpolymers.com All Rights Reserved