Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.80 MPa | 406 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 8191-60B500 Thermoplastic Vulcanizate
(discontinued **) Product Description: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, PA 12.. |