Mechanical Properties Metric English Comments
Tensile Strength at Break 15.7 MPa
2280 psi
ISO 37
PolyOne OnFlex™ V 3040D-S0093 Thermoplastic Elastomer (TPE)
OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef..
Tensile Strength at Break 15.7 MPa
2280 psi
NEU NeuSoft™ 597-60A Industrial Ether TPU / SBC blend
Tensile Strength at Break 15.7 MPa
2280 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R111AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 15.7 MPa
2280 psi
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 90057 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Tensile Strength at Break 15.7 MPa
2280 psi
After 70hrs @347°F in Stauffer 7700
Greene Tweed FLUORAZ® 799 Fluoroelastomer, FEPM
Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f..
Tensile Strength at Break 15.7 MPa
2280 psi
ISO R 527
Stir SpA SR 88 (PVC)
Application: Primary type R 2Information provided by STIR SpA
Tensile Strength at Break 15.7 MPa
2280 psi
ASTM D638
3M Scotchkote™ HB 850 Epoxy Floor Coating
Scotchkote Epoxy Floor Coating HB 850 has been specifically developed as a 100% solids protection system for application to a wide rage of floor surfaces.Product Features:Combines good application c..
Tensile Strength at Break 15.7 MPa
2280 psi
ASTM D638
Teknor Apex APEX® 82-E378-H Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Features: Flame Retardant Uses: Cable Jacketing Agency Ratings: UL 62 Wire Types: SJT; ST; VW-1 Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 15.7 MPa
2280 psi
5mm/min; ASTM D638
Mitsui TPX® MX002 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Copyright © lookpolymers.com All Rights Reserved