Polymer Property : Tensile Strength at Break = 2420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.7 MPa
2420 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne
Tensile Strength at Break 16.7 MPa
2420 psi
5mm/min; ASTM D638
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade  (discontinued **)
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Tensile Strength at Break 16.7 MPa

@Temperature 145 °C,
Time 2100 sec
2420 psi

@Temperature 293 °F,
Time 0.583 hour
cured; ASTM D412
LG Chemical BR 1208 Polybutadiene Polymer
Description: BR1208 is high cis- 1,4 polybutadiene polymer produced by a solution polymerization process employing a stereospecific catalyst to control microstructure, molecular weight and molecular..
Tensile Strength at Break 16.7 MPa

@Temperature 145 °C,
Time 2100 sec
2420 psi

@Temperature 293 °F,
Time 0.583 hour
cured; ASTM D412
LG Chemical BR 1280 Polybutadiene Polymer
BR 1280 is high cis- 1,4 polybutadiene polymer produced by a solution polymerization process polymerization process employing a stereospecific catalyst to control microstructure, molecular weight an..
Tensile Strength at Break 16.7 MPa
2420 psi
ASTM D638
Lotte Chemical Titan TITANZEX® HI1100 High density polyethylene
HI1100 is a non UV stabilised high density polyethylene for injection molding. HI1100 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 ..
Tensile Strength at Break 16.7 MPa
2420 psi
ASTM D638
Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene
HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Ap..
Tensile Strength at Break 16.7 MPa
2420 psi
ASTM D638
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer
Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified ..
Tensile Strength at Break 16.7 MPa
2420 psi
ASTM D412
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..