Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.4 MPa | 2530 psi | |
NEU NeuSoft™ 602-50A Ester TPU / SBC blend |
|||
Tensile Strength at Break | 17.4 MPa | 2530 psi | ASTM D638 |
Teknor Apex APEX® 88-N131M-NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 17.4 MPa | 2530 psi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5642 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5642 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Tensile Strength at Break | 17.4 MPa | 2530 psi | ASTM D638 |
Teknor Apex APEX® 84132 Polyvinyl Chloride, Flexible Notes: 80°C Insulation and Jacketing; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |