Polymer Property : Tensile Strength at Break = 26.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.9 MPa
3900 psi
2 in/min; ASTM D638
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 26.9 MPa
3900 psi
2 in/min; ASTM D638
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black
Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 26.9 MPa
3900 psi
2 in/min; ASTM D638
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 26.9 MPa
3900 psi
2 in/min; ASTM D638
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 26.9 MPa
3900 psi
chs 2 in/min; ASTM D638
Network Polymers NPS 90-0802 Polystyrene
Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc.
Tensile Strength at Break 26.9 MPa
3900 psi
2 in/min; ASTM D638
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
LyondellBasell Petrothene® LB5604 High Density Polyethylene
ApplicationsThe PETROTHENE LB 5604 series of polyethylene resins exhibits good stiffness and environmental stress cracking resistance. Typical applications include household chemical and person car..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
LyondellBasell Petrothene® LB560401 High Density Polyethylene
ApplicationsPetrothene LB560401 exhibits good stiffness and environmental stress crack resistance. Typical applications include household chemical and personal care product bottles.Regulatory Status..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
ITW Devcon Metal Repair Ceramic Repair Putty, Dark Blue
Information provided by ITW Devcon
Tensile Strength at Break 26.9 MPa
3900 psi
Taiwan PU Corporation UR50 Polyester Urethane Rubber
UR50 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of ..
Tensile Strength at Break >= 26.9 MPa
>= 3900 psi
ASTM D412 Method A
Seals Eastern 7345 Highly Saturated Nitrile Rubber
HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength at Break 26.9 MPa

@Temperature 100 °C,
Time 252000 sec
3900 psi

@Temperature 212 °F,
Time 70.0 hour
ASTM D865
Seals Eastern 7345 Highly Saturated Nitrile Rubber
HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc.
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Chase Plastics CP Pryme® N300STL (COND, 50% RH) Nylon 6 (Utility Grade), Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.
Tensile Strength at Break 26.9 MPa
3900 psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Dow DMDA-8940 NT 7 High Density Polyethylene Resin
DOW DMDA-8940 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D2370
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)
3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638 Die C
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638 Die C
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638 Die C
3M Scotch-Weld™ TE031 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D638
Chase Plastics CP Pryme® PPC100-35M Polypropylene Copolymer
Information provided by Chase Plastics.