Mechanical Properties Metric English Comments
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
PolyOne OnForce™ LFT AM-30LCF/001 Grey Polyphthalamide (PPA)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep ..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Amodel® FC -1160 Polyphthalamide (PPA), 60% Glass Fiber
Amodel® FC-1160 is an FDA-approved, 60% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Strength at Break 280 MPa
40600 psi
ISO 527-2
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
Tensile Strength at Break 280 MPa
40600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LX09404 PEEK
LNP* THERMOCOMP* LX09404 is a compound based on Polyetheretherketone resin containing Carbon Fiber.
Tensile Strength at Break 280 MPa
40600 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65
Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya..
Tensile Strength at Break 280 MPa
40600 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65
Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami..
Tensile Strength at Break 280 MPa
40600 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60
Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following ..
Tensile Strength at Break 280 MPa
40600 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65
Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I..