Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Resirene Resirene® 6220 High Impact Polystyrene Features:Low FlowEasy ProcessingGood GlossHigh ElongationFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Extrusion/ ThermoformingDisposablesGPPS/HIPS BlendsRefrigerator PartsInformation p.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638 |
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey Information provided by ITW Devcon |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Teknor Apex APEX® 3701-90NT Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Teknor Apex APEX® 65290 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Good UV Resistance Uses: Communication Wire Jacketing Forms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 80.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Teknor Apex APEX® 80458 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Teknor Apex APEX® 80853-C Polyvinyl Chloride, Flexible Notes: 105°C, Non-lead Stabilized, Insulation; PVC Insulation intended for use in 90°C wet locations; RoHS CompliantFeatures: Flame Retardant; Oil Resistant Uses: Insulation; Wet Rated Insulat.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Teknor Apex Flexalloy® 9607-96 Polyvinyl Chloride, Elastomer Notes: 105°C Jacket; RoHS Compliant Uses Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Teknor Apex APEX® 80853-B Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; Oil Resistant Uses: Insulation; Wire and Cable Applications Agency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire T.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2375A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Teknor Apex Synres® SR 4321 Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D412 |
Teknor Apex Telcar® TL-1427A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
PlastxWorld DAICEL STYROL® GH10 HIPS High heat resistance and flame retarded HIPS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Chase Plastics CP Pryme® PPC300NB-10M Utility Polypropylene Copolymer Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638 |
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Amco Amalloy® B9714 Polymer Alloy Amco Amalloy B9714 is a clear performance copolymer with exceptional clarity and toughness.High elongation before breakage, good melt Flow.Information provided by Amco Plastic Materials. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Americas Styrenics EB6755 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Americas Styrenics STYRON A-TECH® 1400AS High Impact Polystyrene Product CharacteristicsHigh FlowGood ImpactFood Contact CompliantTypical ApplicationsTelevision housingsPrinter HousingsConsumer goodsInformation provided by AmericasStyrenics LLC. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R349AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | ASTM D638 |
Resirene Resirene® 8450 High Impact Polystyrene (Chemical Resistant) Features:Low FlowChemical ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingRegistration LinersExtruded SheetInformation provided by US distributor Calsak Co.. |
|||
Tensile Strength at Break | >= 21.4 MPa | >= 3100 psi | ASTM D882 |
M. Holland Company MAGMA® LL1092-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Tensile Strength at Break | 21.4 MPa | 3100 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W2413 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |