Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 3290 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.7 MPa
3290 psi
Across Flow; DIN 53504
PolyOne OnFlex™ U 5365A-E0134 FG Thermoplastic Elastomer (TPE)
OnFlex™ U 5365A-E0134 FG is a performance TPU alloy designed for use in injection molding application where FDA compliance and Overmolding onto PC, ABS and PC/ABS substrates are required.Properties..
Tensile Strength at Break 22.7 MPa

@Treatment Temp. 145 °C,
Time 2100 sec
3290 psi

@Treatment Temp. 293 °F,
Time 0.583 hour
Cure; ASTM D412
Styron Buna® SB 1739 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Composition: Buna® SB 1739 – Schkopau is manufactured by cold polymerization using mixed rosin acid /fatty acid soaps. In relation to solid rubber it is plasticized with 37.5 parts of TDAE o..
Tensile Strength at Break 22.7 MPa
3290 psi
ASTM D3759
3M 235 Photographic Tape
3M™ Photographic Tape 235 is a black colored opaque tape used in general purpose camera applications.Information provided by 3M
Tensile Strength at Break 22.7 MPa
3290 psi
Post cure 2 hours @ 232°C
3M Dyneon™ FPO 3740 Fluoroelastomer
3M™ Dyneon™ FPO 3740 is a peroxide curable fluoroelastomer terpolymer containing 69.5 wt% fluorine. FPO 3740 can be used in compression, transfer or injection molding, and extrusion processes. Fea..
Tensile Strength at Break 22.7 MPa
3290 psi
Asahi Glass Fluon® RB1020S 20% Glass Fiber, PTFE Filled Compound
Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.
Tensile Strength at Break 22.7 MPa
3290 psi
ASTM D3756
3M 1900 Specialty High Temperature Masking Tape
3M™ Value Duct Tape 1900 is a conformable cloth duct tape made with polyethylene film over cloth scrim and rubber adhesive. A good choice for non-critical applicationsInformation provided by 3M