Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 4.48 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.48 MPa
650 psi
Reinforced Material, warp; ASTM D412
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Tensile Strength at Break 4.48 MPa

@Temperature 23.0 °C
650 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ D3202-1000-03 Thermoplastic Elastomer (TPE)
Dynaflex™ D3202-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -..
Tensile Strength at Break 4.48 MPa
650 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9082 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Strength at Break 4.48 MPa
650 psi
Reinforced Material, warp; ASTM D412
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Tensile Strength at Break 4.48 MPa
650 psi
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate
GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC
Tensile Strength at Break 4.48 MPa
650 psi
Typical for 70 lb/ft³
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall..
Tensile Strength at Break 4.48 MPa
650 psi
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c..
Tensile Strength at Break 4.48 MPa
650 psi
GrafTech GRAFOIL® GTX Standard Fluid Sealing Graphite, Single Layer Material
GRAFOIL® GTX flexible graphite sheet is inhibited for high oxidation/corrosion resistance that can be used for most fluid sealing and industrial applications. Grade GTX contains an inorganic, non..
Tensile Strength at Break 4.48 MPa
650 psi
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material
GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â..
Tensile Strength at Break 4.48 MPa

@Time 7200 sec
650 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarGrip GP 45-1000 TPE
Product Description: StarGrip GP 45-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery..
Tensile Strength at Break 4.48 MPa
650 psi
ASTM D412
Teknor Apex Monprene® MP 1227D Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 4.48 MPa
650 psi
ASTM D412
Teknor Apex Telcar® TL-1081B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 4.48 MPa
650 psi
20 in/min; ASTM D412
Teknor Apex Uniprene® UN-1011A Thermoplastic Elastomer
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Tensile Strength at Break 4.48 MPa

@Temperature 150 °C,
Time 605000 sec
650 psi

@Temperature 302 °F,
Time 168 hour
in Air; ASTM D573
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Copyright © lookpolymers.com All Rights Reserved