Polymer Property : Tensile Strength at Break = 406 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.80 MPa
406 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 8191-60B500 Thermoplastic Vulcanizate  (discontinued **)
Product Description: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, PA 12..