Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.90 MPa | 421 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Tensile Strength at Break | 2.90 MPa @Time 436000 sec |
421 psi @Time 121 hour |
JRF-7 days |
3M AC-240 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Tensile Strength at Break | 2.90 MPa @Time 436000 sec |
421 psi @Time 121 hour |
JRF-7 days |
3M AC-240 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Tensile Strength at Break | 2.90 MPa @Time 436000 sec |
421 psi @Time 121 hour |
JRF-7 days |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |