Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-101 |
SGL Carbon Group SIGRAFIL C® C25 M350 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-103 |
SGL Carbon Group SIGRAFIL C® C25 P250 EPY Pelletized Carbon Fiber, Epoxy Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-104 |
SGL Carbon Group SIGRAFIL C® C25 P350 GLY Pelletized Carbon Fiber, Glycerine Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-102 |
SGL Carbon Group SIGRAFIL C® C25 P350 PUT Pelletized Carbon Fiber, Polyurethane Sizing Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-83 |
SGL Carbon Group SIGRAFIL C® C25 S001 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-81 |
SGL Carbon Group SIGRAFIL C® C25 S003 APS Staple Carbon Fiber, Aromatic Polymer Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-84 |
SGL Carbon Group SIGRAFIL C® C25 S003 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-88 |
SGL Carbon Group SIGRAFIL C® C25 S003 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-79 |
SGL Carbon Group SIGRAFIL C® C25 S003 PUT Staple Carbon Fiber, Polyurethane Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-82 |
SGL Carbon Group SIGRAFIL C® C25 S006 APS Staple Carbon Fiber, Aromatic Polymer Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-85 |
SGL Carbon Group SIGRAFIL C® C25 S006 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-89 |
SGL Carbon Group SIGRAFIL C® C25 S006 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-80 |
SGL Carbon Group SIGRAFIL C® C25 S006 PUT Staple Carbon Fiber, Polyurethane Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-86 |
SGL Carbon Group SIGRAFIL C® C25 S009 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-90 |
SGL Carbon Group SIGRAFIL C® C25 S009 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-87 |
SGL Carbon Group SIGRAFIL C® C25 S012 EPY Staple Carbon Fiber, Epoxy Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-91 |
SGL Carbon Group SIGRAFIL C® C25 S012 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-99 |
SGL Carbon Group SIGRAFIL C® C25 M100 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Tensile Strength at Break | 3600 MPa | 522000 psi | ASTM D3379-100 |
SGL Carbon Group SIGRAFIL C® C25 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |