Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 600 MPa | 87000 psi | Longitudinal |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Tensile Strength at Break | 600 MPa | 87000 psi | Transverse |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Tensile Strength at Break | 600 MPa | 87000 psi | |
Goodfellow Copelmet® Tungsten 72/Copper 28 Alloy Developed as an electrode material, this alloy is used for spark erosion electrodes and contacts giving excellent resistance to mechanical wear and electrical erosion.Information provided by Goodfel.. |
|||
Tensile Strength at Break | 600 - 760 MPa | 87000 - 110000 psi | |
ThyssenKrupp PAS 550 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |