Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 7.58 MPa | >= 1100 psi | ASTM D412 |
S&E Specialty Polymers GPE2001E-ROHS PVC GPE2001E-ROHS flame retardant polyethylene compound designed for wire and cable applications. GPE2001E-ROHS complies with RoHS requirements. GPE2001E-ROHS is suitable for 75°C continuous use and 10.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D1414 |
Greene Tweed Xyfluor® 870 Fluorinated Elastomer Compound Xyfluor® 870, a highly fluorinated elastomer compound, provides excellent chemical compatibility over a wide range of temperatures from -76°F to 450°F (-60°C to 232°C). Recommended f.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | |
Taiwan PU Corporation UR90 Polyester Urethane Rubber UR90 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | |
Shin-Etsu Silicones KE-5560U Low Temperature Silicone Elastomer ShinEtsu KE5560 U is a nominal 60 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1843L1 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1627L3 Thermoplastic Elastomer Features: Excellent Elastic Recovery; Tough; Good Melt Strength Uses: Strap ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1875 Thermoplastic Elastomer Notes: Water; Clear; Adhesion to Polycarbonate Features: High Coefficient of FrictionInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1627 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1881B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2212A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2560B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2770L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
Teknor Apex Telcar® 90-E607D-88NT Ethylene Vinyl Acetate Copolymer Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-1336G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-2590F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow GRSN-9820 NT 7 Linear Low Density Polyethylene Granular Solid DOW GRSN-9820 NT 7 is produced using UNIPOL™ PE process technology and is supplied in granular form. This resin is specifically designed as a carrier resin for color concentrates and other master .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | |
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ISO 37 |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |