Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.64 MPa @Temperature 23.0 °C |
1110 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Tensile Strength at Break | 7.64 MPa @Temperature 23.0 °C |
1110 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |