Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 70.3 MPa | 10200 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 1200 A UV White 205 Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 1200 A L Natural Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)
(discontinued **) Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used .. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
PlastxWorld CEVIAN® B5722 10% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
PlastxWorld CEVIAN® S1210 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Chase Plastics CP Pryme® NN213GL (COND, 50% RH) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
TPI Porene® AS 121 PC (Blue) General Purpose SAN Porene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Tensile Strength at Break | 70.3 MPa @Temperature 22.8 °C |
10200 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Tensile Strength at Break | 70.3 MPa | 10200 psi | ASTM D638 |
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |