Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 79.3 MPa | 11500 psi | 2 in/min; ASTM D638 |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t.. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM-D638 |
Ineos ABS Lustran® SAN DN79 SAN Grade Lustran® SAN DN79 is a natural color, styrene-acrylonitrile copolymer supplied in pellet form. It is designed for used in compounding. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
Plastics Group Polifil® 930L Nylon 6 (DAM) Polifil® NYLON 6 provides superior strength and rigidity with electrical resistance and surface lubricity.Applications: AutomotiveHousingsBearingsAppliances Standard processing techniques are appli.. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
Chase Plastics CP Pryme® NN300HL (Dry) Nylon 66, Heat Stabilized, Lubricated Features: General purposeHeat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Tensile Strength at Break | 79.3 MPa | 11500 psi | ASTM D638 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |