Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.70 MPa @Strain 100 % |
682 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Stress | 4.70 MPa @Strain 100 % |
682 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |