Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant FeaturesModified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfil.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 T 15 MI PA66, 15% mineral filling FeaturesPA 66 with the content of 15 % chemically modified mineral filling and impact modified. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produc.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 1.00 - 1.50 J/cm² @Temperature 23.0 °C |
4.76 - 7.14 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact Unnotched | 1.00 - 1.40 J/cm² @Temperature 23.0 °C |
4.76 - 6.66 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Charpy Impact Unnotched | 1.00 - 1.20 J/cm² @Temperature 23.0 °C |
4.76 - 5.71 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
|
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
|
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
|
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Krasten® 137 General Purpose Polystyrene Easy flow. Examples of Application:Injection moulding – cups and containers for the food industry, medical devices, drawing templates.Extrusion – coextrusion, high gloss surface.Synthos wa.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Krasten® 154 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -20.0 °C |
4.76 ft-lb/in² @Temperature -4.00 °F |
|
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |