Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -20.0 °C |
35.7 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre FeaturesChemically reinforced with 40% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -20.0 °C |
35.7 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RCF3505 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-PG2U (Cond.) 13% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K230-HXG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free Information Provided by LG Chem |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 179-1eU |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 136F4Q32 Nylon 6, 20% Glass Fiber SAXAMID 136F4Q32 is a high impact-modified polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
DSM Akulon® K224-G6-FC NA99001 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM Akulon® K224-LG6 /E PA6-GF30 30% Glass Reinforced, Injection Molding, Improved UV-stability |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® S223-HG7 Nylon 66-35% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG6U PA6, 30% Glass Fiber Filled, UV Stabilized, Injection Molded Staramide BG6U is an UV Stabilized, 30% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |