Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -20.0 °C |
22.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -20.0 °C |
22.4 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -20.0 °C |
22.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature 23.0 °C |
22.4 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A RV300AF (dry) Nylon 66-30GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature 23.0 °C |
22.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1fU |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1fU |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature 23.0 °C |
22.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -20.0 °C |
22.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |