Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® E309 ABS Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® HH-112 ABS Novodur HH-112 is a high heat injection molding grade. It provides good heat resistance combined with enhanced stiffness.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® M201AS ABS Novodur M201AS is a medium impact, high gloss injection molding grade with improved chemical resistanceInformation provided by Styrolution |
|||
Charpy Impact Unnotched | <= 14.0 J/cm² @Temperature -30.0 °C |
<= 66.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Polystyrol 485 I GR 2 PS Description: Polystyrol 485 I GR2 is a high-impact grade of polystyrene for extruded sheets with a matt surface.Applications: Sheet, semi finished goods, fat resistant food packaging.Information pro.. |
|||
Charpy Impact Unnotched | <= 14.0 J/cm² @Temperature -30.0 °C |
<= 66.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Polystyrol ESCRimo PS Description: Polystyrol ESCRimo is a high-impact polystyrene grade with an improved stress cracking resistance compared to conventional high-impact polystyrene.Applications: Due to its superior envi.. |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature -30.0 °C |
66.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2005/1 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Charpy Impact Unnotched | 14.0 J/cm² @Temperature 23.0 °C |
66.6 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |