Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 1305 000000 PBT PBT, non-reinforced, injection molding |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 1505 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® H604 ABS Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® H701 ABS Novodur H701 is an injection molding grade of ABS with heat resistance and high impact strength.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Styrolution Novodur® P2M-AT ABS Pellets Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Novodur® 5300 ABS Novodur 5300 is a high heat injection molding grade with high impact strength, good chemical resistance and reduced emission (PC modified)Information provided by Styrolution |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2001 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® W2320 0035 LEV POM Description: Is a POM, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultraform® W2320 0035 LEV POM Description: Is a POM, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |