Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 34.5 MPa @Temperature 25.0 °C |
5000 psi @Temperature 77.0 °F |
Composite double overlap shear |
Henkel Hysol EA 9695 Film Adhesive Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 ps.. |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature 25.0 °C |
5000 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9309.3NA Paste Adhesive System Toughened adhesive with excellent peel strength. Contains glass beads for bond line control.Applications: Structural Repair Composite Bonding |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature -55.0 °C |
5000 psi @Temperature -67.0 °F |
Lap Shear |
Henkel Hysol PL 777-1FR Film Adhesive Flame retardant, nonmetallic modified epoxy film adhesiveApplications: Metal and Honeycomb Bonding |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature 25.0 °C |
5000 psi @Temperature 77.0 °F |
Lap Shear |
Henkel Hysol PL 777-1FR Film Adhesive Flame retardant, nonmetallic modified epoxy film adhesiveApplications: Metal and Honeycomb Bonding |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature 25.0 °C |
5000 psi @Temperature 77.0 °F |
Lap Shear |
Henkel Hysol EA 9257 Primer Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Visc.. |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature -55.0 °C |
5000 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9330 Paste Adhesive System Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature 25.0 °C |
5000 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9330 Paste Adhesive System Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature 25.0 °C |
5000 psi @Temperature 77.0 °F |
Lap Shear |
Henkel Hysol EA 9657 Film Adhesive High temperature, service film adhesive designed for high honeycomb peel in a reticulated sound suppression structure. Qualified to BMS 5-137. Data from .080 psf, 400 g / m2.Applications: Composite .. |
|||
Adhesive Bond Strength | 34.5 MPa @Temperature 25.0 °C |
5000 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9394/C-2 Paste Adhesive System Elevated cure, thixotropic adhesive with structural properties to 450°F / 232°C.Application: Structural Repair |