Polymer Property : Izod Impact, Unnotched (ISO) = 129 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 129 kJ/m²
61.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific)
LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 129 kJ/m²
61.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU
LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber.
Izod Impact, Unnotched (ISO) 129 kJ/m²
61.4 ft-lb/in²
Goodfellow TPX® MX002O Polymethylpentene
This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi..