Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4413 PC Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ZLL12CP PC (Europe-Africa-Middle East) Medium viscosity general purpose flame retardant polycarbonate grade based on recycled material. Rated UL94 V2 at 1.5 mm. Limited color availability. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 80.0 kJ/m² | 14.3 - 38.1 ft-lb/in² | Average value: 52.4 kJ/m² Grade Count:45 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 100 kJ/m² | 14.3 - 47.6 ft-lb/in² | Average value: 68.2 kJ/m² Grade Count:13 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 60.0 kJ/m² | 14.3 - 28.6 ft-lb/in² | Average value: 47.2 kJ/m² Grade Count:10 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM HU2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MF0044E PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF0044E is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include: Non-Halogen Flame Retardant, Easy Molding.This data was supplied .. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RFB53U PA 66 (Europe-Africa-Middle East) LNP*THERMOCOMP*RFB53U is a compound based on PA 66 resin containing Glass Bead, Glass Fiber. Added features include: UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle E.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Asia Pacific) PPE+PS blend. 10% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including wate.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² @Temperature -40.0 °C |
14.3 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1U |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT 403 M-G0 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 55.0 kJ/m² | 14.3 - 26.2 ft-lb/in² | Average value: 39.4 kJ/m² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 79.0 kJ/m² @Temperature -40.0 - -30.0 °C |
14.3 - 37.6 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 45.7 kJ/m² Grade Count:22 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180/U |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |