Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC
LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by ..
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC
LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI
LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific)
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi..
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12
LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer
LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF0335 PC (Europe-Africa-Middle East)
LNP* Lubricomp* LEXAN_LF0335 compound is a 35% glass fiber, milled glass reinforced PC injection moulding resin with improved wear resistance and reduced friction.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS
LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA
LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT
LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature -30.0 °C
18.1 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON MD000AP PP
LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET
LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer
LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RF0039S PA 66
LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RFB33 PA6.6 (Europe-Africa-Middle East)
LNP*THERMOCOMP* RFB33 is a compound based on PA66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DE003M PC
LNP* STAT-KON* DE003M is a compound based on Polycarbonate containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® SHF4340 PBT
20% GF Super High Flow PBT
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp RFB53SUZ PA 66
LNP THERMOCOMP* RFB53SUZ is a compound based on Nylon 66 resin containing Glass Bead, Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for th..
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66
LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT
LNP THERMOCOMP* WF008 is a compound based on PBT resin containing 40% Glass Fiber.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp XF006S
LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region..
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA
LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
ASTM D256
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC
LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Izod Impact, Unnotched (ISO) 38.0 - 38.0 kJ/m²

@Temperature -30.0 - -30.0 °C
18.1 - 18.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 38.0 kJ/m² Grade Count:1
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp GL004 PSU
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re..