Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 219 kJ/m² | 104 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP GX07409H PSU LNP* LUBRICOMP* GX07409H is a compound based on PSU resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 219 kJ/m² @Temperature 23.0 °C |
104 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp GX07409X PSU Wear resistant PSUThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 219 kJ/m² | 104 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON SD000 PA12 LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive. |