Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 compound |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific) LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WH0450EX PBT (Asia Pacific) LNP* Thermocomp* WH0450EX is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT (Asia Pacific) LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | |
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | |
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1C |
Chi Mei Polyrex® PG-383 Polystyrene High heat; high strength |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1C |
Chi Mei Polyrex® PG-80 Polystyrene High strength |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | Typical; ISO 180 |
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co.. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² | 4.28 ft-lb/in² | ISO 180/1U |
A.D. Compound Adene NTQA Homopolymer 40% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² - NB @Temperature -20.0 - -20.0 °C |
4.28 ft-lb/in² - NB @Temperature -4.00 - -4.00 °F |
Average value: 17.7 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched (ISO) | 9.00 kJ/m² - NB @Thickness 4.00 - 4.00 mm |
4.28 ft-lb/in² - NB @Thickness 0.157 - 0.157 in |
Average value: 17.7 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |