Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180 |
Qualchem Danamid FGF-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² - NB @Temperature -40.0 - -30.0 °C |
28.6 ft-lb/in² - NB @Temperature -40.0 - -22.0 °F |
Average value: 193 kJ/m² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AI0019 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AI0019 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Silicone. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 2nd Grade |
Kazanorgsintez PC-005 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL36 is a compound based on PA 66 resin containing PTFE, Carbon Fiber. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RX05049 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RX05049 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Proprietary Lubricant. Added features include; Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RE004MPC PA 66 LNP* STAT-KON* RE004MPC is a compound based on Nylon 66 resin containing 20% Milled Carbon Fiber. Added features of this material are: Exceptional Processing, Clean Compound System, Electrically C.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP C1000XXP PS (Europe-Africa-Middle East) LNP* THERMOCOMP* C1000XXP is a compound based on Polystyrene resin. Added features include: High Impact. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Europe-Africa-Middle East) LNP* Thermocomp* DF1006 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DFB03GR PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DFB03GR is a compound based on Polycarbonate resin containing a mixture of Glass Fiber and Glass Beads. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66 LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for .. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Europe-Africa-Middle East) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT 403 M-G20 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G25 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G30 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
BLUESTAR 201-G30202 PBT, 30% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 60.0 - 70.0 kJ/m² @Temperature -30.0 - -30.0 °C |
28.6 - 33.3 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 68.0 kJ/m² Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA6 D83 PA6, Injection Molded Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |