Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN
LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A..
Izod Impact, Unnotched (ISO) 8.00 kJ/m² - NB
3.81 ft-lb/in² - NB
Average value: 57.3 kJ/m² Grade Count:30
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON MX01739C PP
LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific)
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific)
LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP MF006AL PP
LNP* THERMOCOMP* MF006AL is a compound based on Polypropylene resin containing 30% Glass Fiber. Characteristics of this grade are: Low Extractable.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MH0255A is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features include; High Specific Gravity.This data was supplied by SABIC-IP for the Europe-..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS
LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180
Polyram PlusTek PD1002NT Nylon 12 for Extrusion
Medium viscosity Nylon 12 for extrusion application.Information provided by Polyram.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding
Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180/1C
Chi Mei Polyrex® PG-80N Polystyrene
High strength
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene
PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS01 3009 Green General Purpose Polystyrene
PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene
PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com..
Izod Impact, Unnotched (ISO) 8.00 - 12.0 kJ/m²
3.81 - 5.71 ft-lb/in²
Spec; ISO 180
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene
PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co..
Izod Impact, Unnotched (ISO) 8.00 - 14.0 kJ/m²
3.81 - 6.66 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene
PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co..
Izod Impact, Unnotched (ISO) 8.00 - 14.0 kJ/m²
3.81 - 6.66 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS01 3000 General Purpose Polystyrene
PS01 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of custom co..
Izod Impact, Unnotched (ISO) 8.00 - 20.0 kJ/m²
3.81 - 9.52 ft-lb/in²
Average value: 16.0 kJ/m² Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Izod Impact, Unnotched (ISO) 8.00 - 129 kJ/m²
3.81 - 61.4 ft-lb/in²
Average value: 43.0 kJ/m² Grade Count:7
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON ME003S PP
LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized.