Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East)
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® MG38U ABS
High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance.
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
ISO 180/1A
Dow INSPIRE™ D7030EZ Thermoplastic Polyolefin  (discontinued **)
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line.
Izod Impact, Notched (ISO) 27.0 - 176 kJ/m²
12.8 - 83.7 ft-lb/in²
Average value: 75.7 kJ/m² Grade Count:8
Overview of materials for High Density Polyethylene (HDPE), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER
LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE
LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas ..
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East)
LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON MV00AS PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, heat stabilized
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
ASTM D256
Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature -50.0 °C
12.8 ft-lb/in²

@Temperature -58.0 °F
Dow LDPE 4012M Low Density Polyethylene
DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and ge..
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermotuf V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific)
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 27.0 kJ/m²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East)
LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON PX06418 PA 6
LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural.
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RX00327 PA 66
LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural.