Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 923 PC (Europe-Africa-Middle East) LEXAN 923 is a low viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD173R PC (Europe-Africa-Middle East) LEXAN FXD173R is a UV stabilized translucent high flow grade for light diffusion special effects. The color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE171R PC (Europe-Africa-Middle East) LEXAN FXE171R is a transparent/translucent high flow grade for special effects colors with a fluorescent appearance. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HF1110 PC (Europe-Africa-Middle East) LEXAN HF1110 is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HF1140R PC (Europe-Africa-Middle East) LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors.Effect.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS1R PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS2R PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® X 408 IN - 10% Talc/Mineral Reinforced Polypropylene Copolymer, Very High Impact Strength & Flow 10% Mineral Reinforced, Very High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180 |
Polyram RamTough PZ126 Polycarbonate, Low Viscosity General purpose, low viscosity polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180 |
Polyram RamLloy PVB702 Nylon/ABS Alloy, Impact Modified Impact modified, UV stabilized Nylon/ABS alloy for injection molding applications.Information provided by Polyram. |