Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 3.00 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound
Izod Impact, Notched (ISO) 3.00 - 47.0 kJ/m²

@Temperature -30.0 - 0.000 °C
1.43 - 22.4 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 15.1 kJ/m² Grade Count:26
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched (ISO) 3.00 - 5.00 kJ/m²
1.43 - 2.38 ft-lb/in²
Average value: 4.22 kJ/m² Grade Count:9
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Grupo Repol Dinalon® B1S25 N Fast Cycling, Nucleated Nylon 6
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP IBI16 PA 6/12
LNP LUBRICOMP* IBI16 is a compound based on Nylon 6/12 resin containing 30% Glass Bead, 2% Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12
LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP
LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant...
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66
LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66
LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA
LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab..
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® 1760 PBT+PC
11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors.
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched
LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -40.0 °C
1.43 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP RB00A PA 66 (Europe-Africa-Middle East)
50% glass beads filled Polyamide 66 injection moulding resin.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp WH0270FX_WH5A289 PBT
2.7 specific gravity PBTThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East)
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Thickness >=5.00 mm
1.43 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Elektro-Isola Etronit IV Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation o..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80x10x4; ISO 180/1A
Eurostar Starpylen MH0200A HDPE, Injection Molding
Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
Addiplast Addinyl B2 K20 Nylon 6
High density and high modulusInformation provided by Addiplast.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead
Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO Test
BASF Ultramid® NFX-0102 NF2004 30% Glass Filled PA66 (Dry)
Ultramid NFX-0102 NF2004 is a heat stabilized, 30% glass bead PA66 injection molding grade. It is especially formulated for low warp, increased stiffness and excellent dimensional stability.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
Addiplast Addinyl A2H M30 Flame Retardant Nylon 66, 30% Mineral Filled
Flame retardant, 30% mineral filled, with halogensInformation provided by Addiplast.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 300 MW4 POM
Mineral filled injection molding grade based on Tarnoform 300 reinforced with 20% wollastonite; such a compound has high stiffness, dimensional stability and hardness combined with low shrinkage.Inf..
Izod Impact, Notched (ISO) 3.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.67 kJ/m² Grade Count:1
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 180/1A
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP
SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I..
Izod Impact, Notched (ISO) 3.00 - 13.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 6.19 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 7.82 kJ/m² Grade Count:32
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.00 kJ/m² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved