Polymer Property : Izod Impact, Notched (ISO) = 3.66 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.70 kJ/m²

@Temperature -40.0 °C
3.66 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
Izod Impact, Notched (ISO) 7.70 kJ/m²
3.66 ft-lb/in²
ISO 180
BASF Ultramid® 66 H2 G/25-V0KB1 NAT 0046 PA66 (Dry)
Information provided by BASF
Izod Impact, Notched (ISO) 7.70 kJ/m²

@Temperature 23.0 °C
3.66 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly..